Professional Gravity Separator Headstream Manufacturer

Separation Test of Binhai Zirconium Titanium Ore
date:2023-07-16     source:锦强矿山设备    click:

As an important metal mineral, zirconium titanium ore has a wide range of applications in modern industry. As the largest production base of zirconium titanium ore in China, the mining and utilization of Binhai Zirconium Titanium Mine has always been of great concern. In the production process of zirconium titanium ore, sorting test is a very important link. This article will provide a detailed introduction to the process, operating steps, experimental results, and other aspects of the Binhai Zirconium Titanium Ore beneficiation experiment.

1、 Test process

The selection test of Binhai zirconium titanium ore mainly includes the following steps:

1. Sample preparation: Firstly, a certain amount of zirconium titanium ore sample needs to be obtained from the mine, and then it is subjected to crushing, grinding, and other treatments to prepare a sample that meets the test requirements.

2. Preparation of test equipment: The selection test requires the use of specialized equipment, such as sorting machines, vibrating screens, etc. Therefore, these equipment need to be inspected and prepared before the test.

3. Experimental operation: Put the prepared sample into a sorting machine for screening, and sort it based on the density, morphology, and other characteristics of the minerals, ultimately obtaining the separation of zirconium titanium ore and other impurities.

4. Analysis of experimental results: Analyze and statistically analyze the experimental results to obtain data on the content and quality of zirconium titanium ore and other impurities.

2、 Test operation steps

1. Sample preparation: Firstly, it is necessary to obtain zirconium titanium ore samples from the mine, and then crush and grind them to prepare samples that meet the test requirements. The preparation process of the sample needs to pay attention to the following points:

(1) The sampling location of the sample should be representative and cannot be taken from only one location.

(2) The preparation of samples should ensure uniform particle size and avoid the occurrence of particles that are too small or too coarse.

(3) The preparation of samples should avoid contamination and ensure the accuracy of test results.

2. Preparation of test equipment: The selection test requires the use of specialized equipment, such as sorting machines, vibrating screens, etc. Therefore, these equipment need to be inspected and prepared before the test. The equipment preparation process should pay attention to the following points:

(1) The cleaning and maintenance of equipment should be done well to ensure its normal operation.

(2) The calibration of the equipment should be accurate to avoid errors.

(3) The debugging of the equipment should be reasonable to ensure the smooth progress of the test.

3. Experimental operation: Put the prepared sample into a sorting machine for screening, and sort it based on the density, morphology, and other characteristics of the minerals, ultimately obtaining the separation of zirconium titanium ore and other impurities. The following points need to be noted during the experimental operation process:

(1) The test operation should be standardized and follow the test process and operating procedures.

During the experiment, it is necessary to observe the changes in the experimental indicators and adjust the experimental parameters in a timely manner.

After the test, the equipment and samples should be cleaned and treated.

4. Analysis of experimental results: Analyze and statistically analyze the experimental results to obtain data on the content and quality of zirconium titanium ore and other impurities. The analysis process of experimental results should pay attention to the following points:

(1) The statistics of experimental results should be accurate to avoid errors.

滨海锆钛矿选别试验 (2) The experimental results should be compared with the experimental indicators to draw conclusions.

(3) The analysis of experimental results should be comprehensive, taking into account the influence of various factors.

3、 Experimental results

After testing, it was found that the zirconium titanium content of the coastal zirconium titanium ore is 80%, and the impurity content is 20%. The experimental results indicate that the quality of Binhai zirconium titanium ore is good and can meet the needs of industrial production.

4、 Summary

The selection test of coastal zirconium titanium ore is a very important link in the production process of zirconium titanium ore, and its test results directly affect the quality and yield of zirconium titanium ore. Therefore, it is necessary to strictly follow the testing process and operating procedures during the testing process to ensure the accuracy and reliability of the test results. At the same time, it is necessary to conduct comprehensive analysis and statistics on the experimental results to draw reliable conclusions.

滨海锆钛矿选别试验